Phase A | |
Pureact SNDT LO (Innospec) (Sodium cocoyl isethionate (&) stearic acid (&) coconut fatty acid (&) sodium isethionate (&) ethylene/ VA copolymer (&) water (&) titanium dioxide) | 85.00 |
Phase B | |
Soap 80/20 soap blend | 10.00 |
Phase C | |
Pureact WS Conc (Innospec) (Sodium methyl cocoyl taurate) | 1.00 |
Phase D | |
Olive oil | 3.00 |
Phase E | |
Tetrasodium etidronate | 0.50 |
Phase F | |
Havanna Sunset (Arylessence Inc.) | 0.50 |
Procedure | |
Add all components to amalgamator and mix well. Using a plodder, make one pass of the material through a pelletizing screen and then another pass through a refining screen as necessary to mix the ingredients. Transfer material to roll mill and complete one cycle of material. Transfer material to plodder fitted with extrusion head and extrude the material through an extrusion plate to form a bar billet. Cut billet to desired length of bar. Use soap press to stamp bar into final form. | |
More Information | |
Innospec Website: www.innospecinc.com |
Cookies help us to provide you with an excellent service. By using our website, you declare yourself in agreement with our use of cookies.
You can obtain detailed information about the use of cookies on our website by clicking on "More information”.
Copyright © 2024 Rodman Media. All rights reserved. Use of this constitutes acceptance of our privacy policy The material on this site may not be reproduced, distributed, transmitted, or otherwise used, except with the prior written permission of Rodman Media.