Phase A
Deionized water
57.69
Glycerin
8.00
Propylene glycol
2.50
Dipropylene glycol
1.50
Sodium lauroyl sarcosinate (30% active)
13.33
Ammoniun lauryl sulfate (28% active)
13.33
SoftCAT polymer SK-L (Polyquaternium-67)
0.25

Phase B
Mineral oil
2.00
Stearyl alcohol
0.50
Cetyl alcohol
0.50

Phase C
DMDM hydantoin
0.40
Fragrance
q.s.

Procedure
Disperse the SoftCAT SK-L in rapidly agitating, room temperature water. Allow to disperse completely. Once the polymer is dispersed, heat the solution to 60-65˚C until clear. Add the  sodium lauroyl sarcosinate, ammoniun lauryl sulfate, glycerin, propylene glycol and dipropylene glycol to the polymer solution, one at a time, in order, waiting for uniformity before adding the next. Heat entire formulation to 60-65˚C. In a separate container, combine the ingredients of phase B. Heat the ingredients to 60-65˚C until the fatty alcohols are dissolved. At temperature, add the contents of phase B to Phase A with good agitation. Mix thoroughly while cooling at 45˚C. Add the DMDM hydantoin and fragrance. Impregnate cloths with concentrate as desired.