Phase A
Deionized water
34.72
Carbopol 980 (Noveon) (Carbomer)
0.20
PEG 7M
0.20
Ammonium lauryl sulfate, 28% (ALS)
14.00
Ammonium laureth sulfate, 25% (ALES)
40.00
Incronam 30 (Cocamidopropyl betaine)
6.60
Glycerin
1.00
Lustreplex (Croda) (Polyquaternium 70 [and] dipropylene Glycol)
1.42
Crodasone Cystine (Cystine bis-PG-propyl silanetriol)
1.00
Crosilk liquid (Silk Amino Acids)
0.20
Disodium EDTA
0.10
Crothix Liquid (PEG-150 pentaerythrityl tetrastearate [and] PEG-6 caprylic/capric glycerides [and] water)
0.26
Flamenco Gold 220C (Engelhard) (Titanium dioxide [and] Mica)
0.20
Neolone 950 (Rohm & Haas) (Methylisothiazolinone)
0.10

Procedure
Charge beaker with deionized water and begin heating to 60°C. Sprinkle Carbomer 980 in the vortex and mix with strong agitation until it is completely dispersed. Repeat the procedure with PEG 7M. When polymers are completely dispersed, reduce the mixing speed and add the ingredients one at a time while continually mixing but avoiding air entrapment in the batch. When all the ingredients are completely mixed and the batch cools to room temperature, check the pH and viscosity.

Properties
pH: 5.5 ± 0.5; Viscosity: 6800 cps ± 10% (RVT Spindle #5 @ 10 RPM, 25°C)