Phase A
Deionized water
51.90
Propylene glycol
2.00
Syntran PC 5208 (Polyacrylate-15)
8.00

Phase B
Polawax NF (Croda) (Emulsifying wax NF)
7.50
Cetyl alcohol (Protameen)
1.00
Snow White petrolatum (Penreco) (Petrolatum)
8.00
Drakeol 7 Lt. mineral oil (Penreco) (Mineral oil)
11.00
Volpo 10 (Croda) (Oleth-10)
2.00
Brij 72 (Uniqema) (Steareth-2)
0.50

Phase C
Deionized water
6.00
Sodium hydroxide
2.10

Procedure
Add water, propylene glycol and Syntran PC 5208 to vessel and begin heating to 75-80°C. Stir until batch is homogenous. With batch at 75-80°C, individually add each Phase B ingredient to batch. Stir between each addition until homogenous emulsion results. Cool batch to 35°C. In a separate water cooled vessel with high shear stirring prepare Phase C. Caution: Premix will become extremely hot, cool as needed. Slowly add Phase C to batch. Homomix until batch is homogenous and smooth. Appearance: Low viscosity, glossy, white creme. pH = 12.6-12.9.