Phase A
Deionized water
84.00
Carbopol Aqua CC Polymer (Noveon) (Polyacrylate-1 crosspolymer)
1.50
Propylene glycol
2.00
Ammonyx 4B (Stepan )(Stearalkonium choride)
3.45
Lanette 18 (Cognis Corp.) (Stearyl alcohol)
1.25
Myritol 318 (Cognis Corp.) (Caprylic/capric triglyceride)
4.55
Herbess Melocoton MEX-EC0016949 (Mane) (Fragrance)
0.60
Citric acid (50% acid solution)
0.15

Phase B
Lanette 16 (Cognis Corp.)(Cetyl alcohol)
2.20

Phase C
Glydant Plus Liquid (Lonza, Inc.) (DMDM hydantoin, iodopropynyl butylcarbamate)
0.30

Procedure
Weigh deionized water into vessel and add Carbopol Aqua CC Polymer. Add remaining ingredients in phase A in the order shown, ensuring that each ingredient is completely dissolved prior to the addition of next ingredient. Heat to 70°C. Mix phase B ingredients in a separate vessel. Heat to 70°C. Add phase B to phase A and mix completely. Wtih mixing, begin cooling to 45°C. Add ingredients of phase C in order shown. Mix until homogenous while batch cools to 35°C. Adjust pH 4.5-5.0 with citric acid.

More info: Noveon, 9911 Brecksville Rd., Cleveland, OH 44141-3247
Tel: (800)379-5389; Fax: (216) 447-5250 Website:  www.personalcare.noveon.com
blog comments powered by Disqus
  • Take Notice

    Take Notice

    Melissa Meisel , Associate Editor||June 1, 2016
    Packaging trends revolve around trendy artwork, eco-conscious materials—and portability is a plus too!

  • Virtual Reality

    Virtual Reality

    Christine Esposito, Associate Editor||June 1, 2016
    An update on nature-identical ingredients for cosmetics and personal care products.

  • Shiseido Advances in the US

    Shiseido Advances in the US

    Tom Branna, Editorial Director||June 1, 2016
    New facility in Windsor, NJ demonstrates its dedication to the US and other markets outside Japan.