Phase A
SD Alcohol 40
65.04
Amphomer polymer (National Starch) (Octylacrylamide/acrylates/butylaminoethyl methacrylate copolymer)
2.50
DynamX polymer (28% solids) (National Starch) (Polyurethane-14 (and) AMP-acrylates copolymer)
1.80
AMP Ultra PC 2000 (95% active) (Angus Chemical) (Aminomethyl propanol)
0.46
Dow Corning 556 Cosmetic Grade Fluid (Dow Corning) (Phenyl trimethicone)
0.20

Phase B
CAP 40 (app. 2.8 bar) (Propane/butane)
30.00

Procedure
To prepare phase A, dissolve AMP in ethanol and start mixing. While maintaining agitation, slowly sift in the Amphomer polymer. When the polymer is completely in solution, add the DynamX polymer  and silicone with mixing until everything is completely dissolved. Filter and transfer the concentrate  into cans. Charge with propellant, phase B.

Properties
Cloud Point: < -25° C

Notes
Any alteration in the formulation can affect propellant compatibility.

More Information
AkzoNobel, Bridgewater, NJ, (888) 331-6212, Fax: (908) 707-3664
 Email: personalcare.usa@nstarch.com, Website: www.personalcarepolymers.com


blog comments powered by Disqus