Phase A
Deionized water
76.10
Ultrez 10 (Lubrizol) (Carbomer)
0.20
Hispagel 200 NS (Cognis Iberia/Centerchem)
3.00
Cutina GMS-SE (Cognis) (Glyceryl stearate)
1.25
Myrj 59 (Croda) (PEG-100 stearate)
1.00
Tegosoft CT (Evonik) (Capric/caprylic triglyceride)
2.00
Stratagel 500 (Centerchem)
8.00
Preventhelia Solution (Lipotec/Centerchem)
5.00

Phase B
Promulgen D (Lubrizol) (Cetearyl alcohol & ceteareth-20)
2.00

Phase C
Sodium hydroxide (10% solution)
0.75

Phase D
Diocide (Centerchem)
0.70

Procedure
Disperse carbomer in water, mix until uniform. Add remaining phase A ingredients, heat to 80°C. Heat phase B to 80°C. Add phase B to phase A under moderate mixing. Mix for 10 minutes. Begin cool down.  At 50°C, add phase C (batch should be ~ pH 6.5) At 40°C, add phase D ingredients one at a time. Mix until uniform. Discontinue.

More Information
Centerchem, Tel: 203-822-9800, Website: www.centerchem.com