Phase A
Dow Corning EL-8050 ID Silicone Organic Elastomer Blend (Isododecane (and) bis-isobutyl PPG-20 crosspolymer)
67.45
Univul MC 80 (BASF) (Ethylhexyl methoxycinnamate)
7.50
Escalol 587 (ISP) (Octisalate)
5.00
Crodamol GTCC (Croda) (Caprylic/capric triglyceride)
8.00
Cetiol OE (Cognis) (Dicaprylyl ether)
12.00
Dow Corning VM-2270 Aerogel Fine Particles (Silica silylate)
0.05

Procedure
Combine all ingredients except silica silylate in a mixing vessel. Mix at 700 rpm with marine propeller until homogeneous (at least 15 min). Increase mixing speed to 1000 rpm. Add silica silylate very slowly while continuing to mix until uniform.

More Information
Dow Corning Corporation, Tel: (989) 496-6000, Website: www.dowcorning.com/content/personal/
blog comments powered by Disqus
  • Sustainability is Omnipresent

    Sustainability is Omnipresent

    Christine Esposito , Associate Editor||July 1, 2016
    Industry stakeholders convene in New York City for Organic Monitor’s annual event

  • Perceived Perfection

    Perceived Perfection

    Christine Esposito, Associate Editor||July 1, 2016
    From primers to pressed powders, facial cosmetics help create the illusion of a flawless complexion.

  • Preserve & Serve

    Preserve & Serve

    Melissa Meisel , Associate Editor||July 1, 2016
    Suppliers with innovative preservatives provide staying power for formulations.