02.01.12
Phase A | |
Dow Corning 9011 elastomer blend (Dow Corning)(Cyclopentasiloxane and PEG-12 dimethicone u2028crosspolymer) | 10.00u2028 |
Sylvaclear PE1800V (Arizona Chemical) (Polyamide-3) | 1.00 |
Water | 56.50 |
Phenoxyethanol | 0.50 |
Pelemol IN-2 (Phoenix Chemical) (Isononyl isononanoate) | 2.00 |
Liponate IPM (Lipo Chemicals) (Isopropyl myristate) | 2.00 |
DC 200 350 cSt (Dow Corning) (Dimethicone) | 9.00 |
Velvesil Plus (Momentive) (Cyclopentasiloxane/u2028C30-45 alkyl cetearyl dimethicone crosspolymer/ u2028PEG/PPG-20/23 dimethicone) | 1.50 |
Dow Corning 5225C (Dow Corning) u2028(Cyclopentasiloxane & PEG/PPG-18/18 dimethicone) | 4.00 |
Neoheliopan AV (Symrise) (Ethylhexyl methoxycinnamate (Octinoxate)) | 6.00 |
Neoheliopan 357 (Symrise) (Butyl u2028methoxydibenzoylmethane (Avobenzone)) | 1.00 |
Neoheliopan 303 (Symrise) (Octocrylene) | 1.00 |
Sodium chloride | 2.00 |
Glycerin | 1.50 |
Detoxophane/Sulforawhite (Tri-K) (Lipidium u2028sativium sprout extract/water/glycerin/lecithin) | 0.25 |
Nanowhite (Tri-K) (Glutathione mixture) | 0.25 |
Trimoist (Tri-K) (Carnosine/glycine soja sterol mixture) | 0.50 |
Spheron P-1500 (Presperse) (Silica) | 1.00 |
Procedure | |
Combine phase A raw materials under high agitation Add Sylvaclear PE1800V to phase A and begin to heat to 85°C while covered. Premix phase C and begin to heat to 65°C and add dropwise to oil phase (A) under high speed homogenization. Cool to 40°C and add phase D materials one at a time with agitation. | |
Properties | |
Stable for 1 month at 40°C; Passed 3 cycles of freeze/thaw. | |
More Information | |
Arizona Chemical Tech. Service: 912-238-6556 Sales: 800-526-5294 or +31-36-5462-800 www.arizonachemical.com |