Phase A | |
Mineral oil | 2.00 |
Emulsifying wax NF | 3.00 |
Steareth-2 | 2.00 |
Steareth-21 | 2.00 |
Cetyl alcohol | 1.00 |
Iron oxides (CI 77492), isopropyl titanium trilsostearate, synthetic wax | 1.30 |
Iron oxides (CI 77491), isopropyl titanium trilsostearate, synthetic wax | 0.40 |
Iron oxides (CI 77499), isopropyl titanium trilsostearate, synthetic wax | 0.15 |
Titanium dioxide, methicone | 6.50 |
Mica, methicone | 6.50 |
Ethylhexyl palmitate | 5.00 |
Xanthan gum | 0.20 |
Deposilk Q1 Polymer (Air Products & Chemicals/Centerchem) | 1.55 |
Preservative | q.s. |
Phase B | |
Water | 55.40 |
Phase C | |
Water | 12.00 |
Procedure | |
Add all ingredients of phase A to main vessel. Begin mixing and heating to 85°C. In another vessel, add water and begin mixing. Sift xanthan gum into water and allow to fully incorporate. Once uniform, begin mixing phase B to 85°C. Once both vessels reach 85°C, add phase B into phase A with mixing. Mix for three minutes. Reduce heat to 60°C and homogenize for three minutes at 6000 rpm. Prepare phase C by dispersing Deposilk Q1 in water and add to homogenized product. Continue to mix while cooling to 40°C. Homogenize again for three minutes at 6000 prm. Add preservative and mix until batch has cooled to room temperature. | |
More Information | |
Centerchem, Inc. 203-822-9800 Fax: 203-822-9820 Website: www.centerchem.com |