09.27.13
Phase A | |
Deionized water | q.s. to 100 |
Amaze XT polymer (AkzoNobel) (Dehydroxanthan gum) | 1.00 |
Propylene glycol (JT Baker) | 5.00 |
Hydrovance (AkzoNobel) (Hydroxethyl urea) | 5.00 |
Citroflex 2 (Moflex) (Triethyl citrate) | 0.20 |
Phase B | |
Drakeol 10 LT (Penreco) | 2.00 |
Neo Heliopan AV (Symrise) (Ethylhexyl methoxycinnamate) | 7.50 |
Tween 20 (Croda) (Polysorbate 20) | 3.00 |
DC 200/350cps (Dow Corning) (Dimethicone) | 5.00 |
Phase C | |
Cremophor RH-40 (BASF) (PEG-40 hydrogenated castor oil) | 0.50 |
DC-193 (Dow Corning) (PEG-12 dimethicone) | 2.00 |
Glydant Plus Liquid (Lonza) (DMDM hydantoin (and) iodopropynyl butylcarbamate) | 0.50 |
Procedure | |
Fill main vessel with deionized water and begin heating to 75°C. Slowly add the Amaze XT polymer and allow Amaze XT polymer to completely hydrate. Once hydrated, add propylene glycol, Hydrovance moisturizing agent and Citroflex-2 and mix well. Add all ingredients in a separate mixing vessel and heat to 75°C. Once both phase A and phase B have reached 75°C, add phase B to phase A with good mixing, approx.. 300-400rpm. Cool to 45°C. Once phase AB has reached 45°C, add phase C ingredients one at a time to phase AB and allow each ingredient to be incorporated fully before adding the next ingredient. Mix until homogeneous. | |
Properties | |
pH—5.5-6.5; Viscosity—15,000-25,000. | |
More Information | |
AkzoNobel Surface Chemistry Global Personal Care 888-331-6212 Email: personalcare.usa@akzonobel.com www.akzonobel.com/PersonalCare |