05.02.14
Phase A | |
Deionized water | 80.9 |
Zemea (DuPont) (Propanediol) | 3.0 |
Salicat MI 10 (Salicylates and Chemicals) (Methylisothiazolinone) | 0.1 |
Phase B | |
Dow Corning FZ-3196 (Caprylyl methicone) | 4.0 |
Dow Corning 5562 Carbinol Fluid (Bis-hydroxyethoxypropyl dimethicone) | 4.0 |
Emanon EVE (Kao Chemicals) (Glycereth-7 caprylate/caprate) | 6.0 |
Viscolam AT 100 EF (Lamberti) (Sodium polyacryloyldimethyltaurate (and) hydrogenated polydecene (and) caprylyl/capryl glucoside) | 2.0 |
Procedure | |
Combine phase B ingredients and mix until homogeneous. Add phase A slowly to phase B while stirring. Homogenize the emulsion for 5 minutes. | |
More Information | |
Dow Corning Corporation 989-496-6000 • Fax: 989-496-5508 Website: www.dowcorning.com/content/personal |