02.06.15
Phase A | |
Endisil FC-345 (Coast Southwest, Endisil, Inc.) (Cyclopentasiloxane) | 5.00 |
Endisil EM-4518 (Coast Southwest, Endisil, Inc.) (Cyclotetrasiloxane (and) cyclopentasiloxane (and) PEG/PPG 18/18 dimethicone) | 12.00 |
Olivatis 12 (Coast Southwest, Medolla Italia, s.r.l.) (Polyglyceryl-3 pentaolivate) | 8.00 |
Endisil FS-677 (Coast Southwest, Endisil, Inc.) (Phenyl trimethicone) | 1.50 |
Phase B | |
Endimate IPP (Coast Southwest) (Isopropyl palmitate) | 1.50 |
Endipure Shea (Coast Southwest) (Butyrospermum parkii) | 2.00 |
AllyEster (Coast Southwest, Allyson Enterprises, Inc.) (Ethyl palmate) | 1.00 |
Endicare TN (Coast Southwest) (C12-15 Alkyl benzoate) | 2.00 |
Phase C | |
Avis (Coast Southwest, Vivimed Labs USA Inc.) (Butyl methoxydibenzoylmethane) | 2.00 |
Octyne-B (Coast Southwest, Vivimed Labs USA Inc.) (Octocrylene) | 2.50 |
Endisil SPS-7350 (Coast Southwest, Endisil, Inc.) (Cyclomethicone (and) trimethylsiloxysilate) | 1.00 |
Cinnamon (Coast Southwest, Vivimed Labs USA Inc.) (Ethylhexyl methoxycinnamate) | 3.50 |
Phase D | |
Endisil S-1501 (Coast Southwest, Endisil, Inc.) (Cyclomethicone (and) dimethiconol) | 2.00 |
Phase E | |
Deionized water | 43.50 |
Sodium chloride | 0.50 |
Propylene glycol (Coast Southwest) (Propylene glycol) | 3.00 |
Sharomix DMP (Coast Southwest, Sharon Laboratories Ltd.) (Diazolidinyl urea (and) methylparaben (and) propylparaben (and) propylene glycol) | 1.00 |
Phase F | |
Luxscreen TR14 AF 50 (Coast Southwest)(Titanium dioxide (and) hydrogenated polydecene (and) styrene/acrylates copolymer) | 4.00 |
Luxscreen TR35 AF 50 (Coast Southwest) (Titanium dioxide (and) hydrogenated polydecene (and) styrene/acrylates copolymer) | 4.00 |
Procedure | |
Phase A—In main vessel add phase A under shear mixing. Phase B—In separate vessel, add phase B and heat to 50-55°C under agitation. Phase C—Add phase C to phase B separate vessel and continue heat to 75°C under agitation. Once content of separate vessel reaches 75°C and uniformity, discontinue heat and allow to cool to 50°C under agitation. At 50°C add to the main vessel and continue shear mixing. Phase D—Add phase D to main vessel under shear mixing. Phase E—In separate vessel add phase E under agitation. Once uniform, slowly add to main vessel increasing shear mixing speed as necessary so that phase E is incorporated by the vortex and does not rest on the surface of mixture. Continue this technique until phase E is uniformly incorporated into mixture. It is crucial for phase E to be added very slowly. Note: Time this process. Once mixture is uniform, let mix for the same allotted time it took to add to avoid over-shearing. Phase F—Add phase F to main vessel under shear mixing. | |
Properties | |
pH—NA. Viscosity: spindle 2.0 at 5.0 rpm = 6,920 cst. Estimated SPF value available upon request. | |
More Information | |
Coast Southwest, Inc. 800-621-0500 Fax: 714-524-8363 Email: info@coastsouthwest.com Website: www.coastsouthwest.com |