07.01.15
Phase A | |
Deionized water | 68.18 |
Hydrovance moisturizing agent (50% solids) (AkzoNobel) (Hydroxyethyl Urea) | 14.00 |
Purolan TEC (Lanxess) (Triethyl citrate) | 0.35 |
D-Panthenol 75L (DSM Nutritional) (Panthenol (&) water) | 0.67 |
Phase B | |
Cutina GMS-SE (BASF) (Glyceryl stearate SE) | 6.00 |
Lanette O (BASF) (Cetearyl alcohol) | 2.00 |
Pristerene 4916-SO-(GD) (Croda) (Fatty acids, C16-18) | 2.00 |
Tegosoft OS (Evonik) (Ethylhexyl stearate) | 3.00 |
Drakeol 7 (Penreco) (LT mineral oil) | 3.00 |
Phase C | |
Euxyl PE 9010 (schülke & mayr) (Phenoxyethanol (and) ethylhexylglycerin) | 0.80 |
Procedure | |
Phase A: Combine all ingredients with propeller mixing at 500-600 rpm. Heat to 75–80°C. Phase B: Combine all ingredients in a separate vessel and heat to 80°C. Once both phase A and B have reached temp. slowly add phase B to phase A under the homogenizer. Mix for 10 min. at 75°C. Turn off heat. Continue to mix at 500-600 rpm and cool below 45°C. Phase C: Cool to 45°C. Add phase C ingredients and mix well. | |
Properties | |
pH—5.5–6.5; Viscosity—8,000–16,000cps Brookfield RVF, T-Spindle,10 rpm. | |
More Information | |
AkzoNobel Surface Chemistry 800-906-9977 Email: personalcare.usa@akzonobel.com Website: www.akzonobel.com/PersonalCare |