Phase A | |
Lanette O (BASF Corporation) (Cetearyl alcohol) | 4.00 |
Polawax GP-200 (Croda) (Emulsifying wax) | 1.50 |
Phase B | |
Deionized water | 85.50 |
Celquat L-200 polymer (Akzo Nobel) (Polyquaternium-4) | 0.30 |
Structure XL rheology modifier (Akzo Nobel) | |
Hydroxypropyl starch phosphate (AkzoNobel) | 2.00 |
Phase C | |
Armocare VGH-70 (75% active) (AkzoNobel (Dipalmitoylethyl dimonium chloride) | 2.00 |
Dow Corning 1501 Fluid (Dow Corning) (Cyclopentasiloxane (and) dimethiconol) | 2.00 |
Phase D | |
Dow Corning 949 (Dow Corning) (Amodimethicone (and) trideceth-12 (and) cetrimonium chloride) | 2.00 |
Dissolvine NA2-S chelate (AkzoNobel) (Disodium EDTA) | 0.20 |
Euxyl PE 9010 (Schülke & Mayr) (Phenoxyethanol (and) ethylhexylglycerin) | 0.50 |
Procedure | |
Combine all ingredients in Phase A and heat to 80°C. For Phase B, disperse the Structure XL starch and Celquat L-200 polymer into water and heat to 80°C. Keep mixing until all the ingredients are well dispersed. While maintaining the 80°C temperature, add Phase B to Phase A with good agitation. Add Phase C into Phase AB at 70~75°C and then homogenize the batch for at least 10 minutes. Slowly keep mixing at 500 rpm and cool to 40°C. Add all the ingredients of Phase D to Phase ABC. Continue mixing the batch and cool to room temperature. Adjust pH to 4.25 - 4.75 if necessary. | |
Properties | |
Color White—Off-white; Appearance—Opaque cream; pH 3.5 - 4.5; Wiscosity—10,000 - 30,000 cPs. | |
More Information | |
AkzoNobel Surface Chemistry Personal Care 800-906-9977 Fax: 908-707-3664 Email: personalcare.usa@akzonobel.com Website: www.akzonobel.com/PersonalCare |