11.02.15
Phase A | |
Deionized water | 51.25 |
Caffeine Anhydrous (Coast Southwest) (Caffeine) | 0.05 |
Hydrasoft Cushion (Coast Southwest and The Innovation Company) (Glyceryl Polymethacrylate (and) butylene glycol (and) zea mays (corn) starch) | 3.00 |
Roasted Cocoa Barley & Coffee Tea Beverage Concentrate (Coast Southwest and Tea Guys) (Water (and) cane sugar (and) black tea blend (and) cocoa beans (and) coffee beans (and) roasted yerba mate (and) lemon juice (and) roasted chicory (and) barley (and) vanilla (and) sea salt (and) citric acid) | 10.00 |
Olivatis 16 (Coast Southwest, Inc.) (Olea europea (olive) fruit oil (and) helianthus annuus (sunflower) seed oil (and) tocopherol (and) aloe barbadensis leaf extract (and) olive oil glycereth-8 esters) | 3.00 |
Siltext Velvet (Coast Southwest and The Innovation Company) (Hydrogenated polyisobutene (and) dimethicone (and) polyethylacrylate) | 3.00 |
Phase B | |
Pelavie Peat (Coast Southwest and The Innovation Company) (Peat (and) phenoxyethanol) | 10.00 |
Pelavie White Clay (Coast Southwest and The Innovation Company) (Bentonite) | 11.00 |
Phase C | |
Sharomix CP-10 (Coast Southwest and Sharon Laboratories) (Chlorphenesin (and) Phenoxyethanol) | 0.70 |
Phase D | |
Endicare ETP-510 (Coast Southwest) (Sodium polyacrylate (and) hydrogenated polydecene (and) trideceth-6) | 1.50 |
Phase E | |
Fiflow BTX (Coast Southwest, Inc. and The Innovation Company) (Perfluorohexane (and) perfluoroperhydrophenanthrene (and) perfluorodecalin (and) perfluorodimethylcyclohexane) | 5.00 |
Phase F | |
Pumice Stone (Coast Southwest) (Pumice) | 1.50 |
Procedure | |
Phase A–Add phase A to main vessel under shear mixing and heat to 60°C. Note: Allow each material to reach uniformity before adding the next. Phase B–Once at desired temperature, add phase B to main vessel on high shear. Begin cool down. Phase C–When main vessel is below 45°C, add phase C to main vessel under low shear mixing. Phase D–Add phase D to main vessel. Formula will thicken. Phase E–Add phase E to main vessel under high shear mixing. Transfer to homogenizer and homogenize to uniformity. Note: Batch may thicken more. Phase F–Disperse Phase F into batch slowly until uniform. Transfer to final container. | |
Properties | |
pH—5.0 - 5.5; Viscosity—spindle 5.0 at 5.0 rpm = 60,000-75,000 cst. | |
More Information | |
Coast Southwest, Inc. 800-621-0500 • Fax: 714-524-8363 Email: info@coastsouthwest.com Website: www.coastsouthwest.com |