Phase A | |
Xirona Nordic Sunset (Merck/EMD) (Silica (and) titanium dioxide (and) tin oxide) | 13.00 |
Colorona Patina Silver (Merck/EMD)(Mica (and) iron oxides (and titanium dioxide) | 2.00 |
Water, demineralized | 68.00 |
Carbopol Ultrez 12 (Gatteosse) (Acrylates/C10-20 alkyl acrylate crosspolymer) | 0.30 |
Phase B | |
Triethanolamine Emprove exp. (Merck/EMD) (Triethanolamine) | 0.70 |
Preservatives (q.s.) | 1.00 |
Glycerol, anhydrous (Merck/EMD) | 2.00 |
Water, dimeralized | 13.00 |
Procedure | |
Disperse all ingredients in the water of phase A. With stirring, add Carbopol Ultrez 21. Mix with high agitation until thoroughly dispersed. Premix the ingredients in phase B until a homogeneous solution is obtained. Add phase B slowly to phase A while stirring. Adjust the pH to 7.0-7.5 with citric acid, if necessary. | |
More Information | |
EMD Performance Materials 484-652-5600 Email: rona@emdgroup.com Website: www.emdgroup.com/en |