Deionized water | 87.49 |
Gafquat 755N polymer (Ashland) (Polyquaternium-11) | 2.50 |
PVP/VA W-735 (Ashland) (VP/VA Copolymer) | 2.00 |
Carsoquat CT-429 (Lonza) (Cetrimonium chloride) | 0.20 |
Styleze ES-1 polymer (Ashland) (Guar hydroxypropyltrimonium chloride) | 1.00 |
Optiphen preservative (Ashland) (Phenoxyethanol (and) caprylyl glycol) | 0.75 |
Ritalac (Rita) (Lactic acid) | 0.06 |
Hydrocarbon A-46 (Diversified CPC) (Propane (and) Isobutane) | 6.00 |
Procedure | |
Add water and begin mixing. Add ingredients one at a time and mix until uniform. Fill cans while continuing to mix, vacuum crimp and charge with propellant. | |
Properties | |
Description—rich, creamy white mousse; Passed 3 M stability test. | |
More Information | |
Ashland Tel: 877-546-2782 Website: www.ashland.com |