Phase A-1 | |
UV Filter Blend | 30.00 |
Phase A-2 | |
KSG-320 (Isododecane, PEG-15 lauryl dimethicone crosspolymer) | 5.00 |
KF-6038 (Lauryl PEG-9 polydimethylsiloxyethyl dimethicone) | 1.50 |
Dicaprylyl carbonate | 4.00 |
KF-56A (Diphenylsiloxy phenyl trimethicone) | 4.00 |
KSP-102 (Vinyl dimethicone/methicone silsesquioxane crosspolymer) | 4.00 |
Phase A-3 | |
Ozokerite wax | 3.00 |
Polyethylene wax | 7.00 |
Phase B | |
Water | 35.80 |
Glycerin | 5.00 |
Phenoxyethanol | 0.70 |
Procedure | |
In a side kettle combine A1 and heat to 90°C with mixing until solution is clear. Cool down to 25°C. In the main kettle under a dispersing blade, combine A2 and heat to 87-90°C. Add A3 and mix until melted. In a side kettle combine B and heat to 87-90°C. Emulsify by adding B to A under low shear (~450-900 rpm) for 1-2 minutes and then increase speed to ~1600 rpm for 3 minutes. Reduce speed to 500 rpm and mix for 5 minutes. Fill into desired container between 80-85°C. | |
Properties | |
Appearance—Opaque white stick. | |
More Information | |
Shin-Etsu: Tel: 330-630-9860 Website: www.shinetsusilicone-global.com |