Released by Coast Southwest, Inc.
Charles Sternberg, Assistant Editor03.02.21
Phase A | |
Deionized water | 62.20 |
Xanthan gum | 0.50 |
Phase B | |
Kisolite BMP (Coast Southwest Inc./Kisolite Corp.) (Clay) | 15.00 |
Phase C | |
Jojoba oil (Coast Southwest Inc./Jojoba Desert (A.C.S. LTD)) (Simmondsia chinensis (jojoba) seed oil) | 6.00 |
Coconut oil (Coast Southwest Inc./International Cosmetic Science Centre (ICSC)) (Cocos nucifera (coconut) oil) | 6.00 |
Cetearyl alcohol (Coast Southwest Inc.) (Cetearyl alcohol) | 3.00 |
Olivatis 19 (Coast Southwest Inc./Medolla Iberia S.L.) (Olive oil polyglyceryl-6 esters, phospholipids) | 2.50 |
Olivatis 18 (Coast Southwest Inc./Medolla Iberia S.L.) (Olive oil polyglyceryl-6 esters, sodium stearoyl lactylate, cetearyl alcohol) | 4.00 |
Phase D | |
Sharomix Amplify AM25 (Coast Southwest Inc./Sharon-Laboratories Ltd) (Phenoxyethanol, chlorphenesin, caprylyl glycol, didecyldimonium chloride) | 0.80 |
Procedure | |
Phase A – In main vessel with mixing, disperse phase A in DI water. Phase B – Once hydrated, slowly add phase B. The solution will appear discontinuous at first; allow the solution to wet out completely until uniform. Begin heating to 65°C to 70°C. Phase C – In a separate vessel begin heating and mixing phase C to 65°C to 70°C. At 65°C to 70°C, add phase C to phase AB. Increase speed as needed. Avoid introducing air. Once batch is completely uniform, discontinue heat and begin cooling. Phase D – At 40°C, add phase D. Transfer the mixture to holding vessel. Product will continue to thicken. | |
Properties | |
pH—6.5 to 7.5; Viscosity—Spindle 5 @ 20 = 15,000 to 18,000 cp. | |
More Information | |
Coast Southwest Inc. 800-621-0500 info@coastsouthwest.com www.coastsouthwest.com |