Phase A | |
Water | q.s. |
Polyglykol 3350 P (Clariant) (PEG-75) | 1.50 |
Phase B | |
Ethanol – SD 40B 200 | 62.00 |
Phase C | |
Aristoflex Velvet (Clariant) (Polyacrylate Crosspolymer-11) | 1.00 |
Phase D | |
Dye | q.s. |
SilCare Silicone 1M71 (Clariant) (Stearoxytrimethylsilane) | 2.00 |
Procedure | |
Combine components of A, mix until homogenous. Adjust pH to 4.0 – 5.0. Add B while stirring. Add C while stirring, mix until homogenous gel forms. Add D while stirring, one at a time, continue mixing at ~300 rpm until pearlescent and homogenous. | |
Properties | |
Appearance—Pearlized gel; pH—4.0 – 5.0; Viscosity (Brookfield, 20°C 20 rpm)—12,000 – 14,000 mPas. | |
More Information | |
Clariant Corporation Website: www.clariant.com |