Deionized water | 94.15 |
Carbomer | 0.50 |
Intelimer 8600 (Air Products and Chemicals/Centerchem) | 2.10 |
Triethanolamine | 0.75 |
Phenyl trimethicone | 0.50 |
Panthenol | 0.50 |
Cyclopentasiloxane (and) dimethicone | 1.00 |
DMDM hydantoin | 0.50 |
Procedure | |
Disperse Carbomer into water while stirring and gently mix until it is fully dispersed. Add all other ingredients including Intelimer 8600 polymer one by one while stirring and gently mix for 15 to 20 minutes. Fill into desired package. | |