Phase A | |
KSG-710 (Dimethicone (and) Dimethicone/Polyglycerin-3 Crosspolymer) | 5.00 |
KSG-19 (Dimethicone (and) Dimethicone/Vinyl Dimethicone Crosspolymer) | 7.00 |
KF-6104 (Polyglyceryl-3 Polydimethylsiloxyethyl Dimethicone) | 2.00 |
DM-Fluid-A-6cs (Dimethicone) | 0.77 |
DM-Fluid-2cs (Dimethicone) | 7.00 |
Bentone Gel NGD V (Neopentyl Glycol Diheptanoate (and) Disteardimonium Hectorite (and) Propylene Carbonate) | 4.00 |
Isododecane | 3.00 |
Phase B | |
DI Water | 49.63 |
Glycerin | 8.00 |
Sodium Chloride | 0.50 |
Sodium Citrate | 0.20 |
Phase C-1 | |
DM-Fluid-A-6cs (Dimethicone) | 2.70 |
KTP-09 Pigments (Triethoxysilylethyl Polydimethylsiloxyethyl Hexyl Dimethicone (and) Aluminum Hydroxide; CI 77891 (KTP-09W) 8.12%, CI 77492 (KTP-09Y) 1.32%, CI 77491 (KTP-09R) 0.36%, CI 77499 (KTP-09B) 0.20% | 10.00 |
Phase C-2 | |
KP-578 (Acrylates/Ethylhexyl Acrylate/Dimethicone Methacrylate Copolymer) | 0.20 |
Procedure | |
Combine Phase A1 using a dispersing blade and mix until homogenous. In a side vessel, combine Phase B with simple stirring. Emulsify by adding Phase B to Phase A under low shear ~400-900rpm. Then, increase speed to 3,000rpm for 5 minutes. Premix Phase C1 using a three-roller mill. Add Phase C2 to Phase C1 and mix well first, then add to Phase AB around 1,000rpm and mix 1-2 minutes until smooth and uniform. | |
Properties | |
Stability: F/T 3 Cycles (-20°C/RT): Passed. 25°C, 50°C. 3 Months: Passed. Appearance: Medium beige cream. Viscosity: Brookfield RV Spindle 6, Speed 20, 1 min @ 25°C —24 hr ~ 24,250 cp. | |
More Information | |