Lanette O (BASF) (Cetearyl alcohol) | 4.00 |
Phase A | |
Polawax GP-200 (Croda) (Emulsifying wax) | 1.50 |
Phase B | |
Deionized water | 85.50 |
Celquat L-200 polymer (AkzoNobel) (Polyquaternium-4) | 0.30 |
Structure XL starch (AkzoNobel) (Hydroxypropyl starch phosphate) | 2.00 |
Phase C | |
Armocare VGH-70 (75% active) (AkzoNobel) (Dipalmitoylethyl dimonium chloride) | 2.00 |
Dow Corning 1501 Fluid (Dow Corning) (Cyclopentasiloxane (and) dimethiconol) | 2.00 |
Phase D | |
Dow Corning 949 (Dow Corning) Cationic emulsion t(Amodimethicone (and) trideceth-12 (and) cetrimonium chloride) | 2.00 |
Dissolvine NA2-S chelate (AkzoNobel) (Disodium EDTA) | 0.20 |
Euxyl PE 9010 (Schu00c3u00bclke & Mayr GmbH) (Phenoxyethanol (and) ethylhexylglycerin) | 0.50 |
Procedure | |
Combine all ingredients in phase A and heat to 80C. For phase B, disperse the Structure XL starch and Celquat L-200 polymer into water and heat to 80C. Keep mixing until all the ingredients are well dispersed. While maintaining the 80C temperature, add phase B to phase A with good agitation. Add phase C into phase AB at 70~75C and then homogenize the batch for at least 10 minutes. Slowly keep mixing at 500 rpm and cool to 40C. Add all the ingredients of phase D to phase ABC. Continue mixing the batch and cool to room temperature. Adjust pH to 4.25-4.75 if necessary. | |
Properties | |
Color Whiteu0-Off-white; Appearance-Opaque; pH-3.5-4.5; Viscosity-4,500-35,000 cps. | |
More Information | |
AkzoNobel Global Personal Care 888-331-6212 Fax: 908-707-3664 Email: personalcare.usa@akzonobel.com www.akzonobel.com/PersonalCare |