Phase A | |
79.42 | |
Stabyl
en 30 (Coast
Southwest, 3V
Sigma-USA) (Acrylate
s/vinyl isodecanoate
crosspolymer) | 0.85 |
E
ndiquest GLDA (Coast
Southwest)
(Tetrasodium
glutamate
diacetate) | 0.50 |
Phase B | |
5.00 | |
Endicar
e OMC (Coast
Southwest)
(Ethylhexyl
methoxycinnamate) | 7.50 |
U
vasorb MET (Coast
Southwest, 3V
Sigma-USA)
(Benzophenone-3) | 3.00 |
E
ndicare AB (Coast
Southwest) (Butyl
methoxydibenzoylmeth
ane) | 2.00 |
Phase C | |
0.73 | |
Phase D | |
1.00 | |
Procedure< /strong> | Phase A – Add Phase A to main vessel with continuous shear mixing. Note: Disperse polymer slowly. Phase B – In a separate vessel, combine phase B in formula order under continuous mixing while heating to 167˚F to 176˚F (75˚C to 80˚C). Once uniform, add phase B to phase A under shear mixing. Phase C – Add phase C to main vessel under continuous mixing. Phase D – When main vessel is less than 104˚F (40˚C), add phase D with continuous mixing. Homogenize if needed to enhance uniformity. Transfer to final container. |
Properties | pH—5.5 to 6.0; Viscosity—spindle 06 @ 6.0 rpm = 70,000 to 100,000 cst. |
Coast Southwest, Inc. Tel. 800-621-0500 Email: info@coastsouthwest. com Website: www.coastsouthwest.c om |
Cookies help us to provide you with an excellent service. By using our website, you declare yourself in agreement with our use of cookies.
You can obtain detailed information about the use of cookies on our website by clicking on "More information”.
Copyright © 2024 Rodman Media. All rights reserved. Use of this constitutes acceptance of our privacy policy The material on this site may not be reproduced, distributed, transmitted, or otherwise used, except with the prior written permission of Rodman Media.